Just Sculpt Tartaric Acid 1lb.

Article number: 88006
Availability: In stock (11)

Patination Formula For Browning Bronze

  • (Cold process)

    • Ammonium Carbonate (3 parts)
    • Cupric Acetate (1 part)
    • Tartaric Acid in Vinegar (1 part)
    • Sodium Chloride Salt (1 part)
      Note: Make a paste of these ingredients, smooth it over the bronze
      for 1 hour and rinse with hot water.
0 stars based on 0 reviews